April 21Apr 21 Hi all, just joined up. I'm about a zillion years into a 19th C Methodist chapel conversion. All the big stuff was done ages ago and I've loaned my mixer out to a bloke up the road. All the old dried up solid bags of OP and lime have been binned for a while. I've just changed a 1st storey window and need to point up round the frame where it meets the old Norfolk red/Suffolk white bricks. Way back in the day I spent weeks doing trial mixes with mortar to get a match on the original lime mortar, but that was when I was laying bricks too. I just need literally a shovel full or so of mortar, if that, so I wondered what the modern premixed stuff was like? I'd be very interested to hear what people might have to say/suggest/recommend/warn about! Thanks in advance - I've attached a couple of snaps to paint the picture. Cheers, Geoff
April 21Apr 21 Ive found it great. You can send a sample off and they will match it for you too. If you are exposed, you might want to add some pozzlan, but given you loction, i guess that doesnt apply?
April 22Apr 22 Have you tried a small mix of whatever sand you get locally and some NHL 3.5 at around 3:1? might be just the ticket!
April 22Apr 22 Author 15 hours ago, Roger440 said: Ive found it great. Hi Roger, thanks for the reply - but I'm not sure what the 'it' refers to!! Geoff
April 22Apr 22 Author 3 hours ago, jfb said: Have you tried a small mix of whatever sand you get locally and some NHL 3.5 at around 3:1? might be just the ticket! Hi, there's a lot of different sands available, as with the lime, but I'm trying to avoid a couple of scarcely used big bags of material sitting and going off!
April 23Apr 23 On 22/04/2026 at 10:54, geoffmuller said: Hi Roger, thanks for the reply - but I'm not sure what the 'it' refers to!! Geoff Premixed lime putty.