Hi all,  has anyone any experience of inclusion rates of perlite in hyd lime/sand render?
 
	application is internal wall insulation pre bonding coat, pre wood fibre insulation.
 
	 
 
	the notion is to lift/soften the dew point and raise U by a small degree as am achieving fairly low value with just the wood fibre board, however have plenty of `U` to trade on roof and floor and quoted L15.1 b. 
 
	 
 
	Thanks, Nick